Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall UV-6685 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall UV-6685 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D-2240
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D-638
Tensile Modulus 2.28 GPa
330 ksi
ASTM D-638
Flexural Strength 53.8 MPa
7800 psi
ASTM D-790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D-790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.30 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
4.54 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
8.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.00 °C
154.4 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D-648
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 240
Georgia Gulf Test
Users viewing this material also viewed the following: