Material Notes:
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing.Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ASTM D2240
Tensile Strength, Ultimate 33.0 MPa
4790 psi
ASTM D412
Tensile Strength, Yield 7.60 MPa

@Strain 100 %
1100 psi

@Strain 100 %
ASTM D-412
12.0 MPa

@Strain 300 %
1740 psi

@Strain 300 %
ASTM D-412
Elongation at Break 640 %
640 %
ASTM D412
Modulus of Elasticity 0.0250 GPa
3.63 ksi
Poissons Ratio 0.25
0.25
Calculated
Shear Modulus 0.0100 GPa
1.45 ksi
Tear Strength 105 kN/m
599 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 30
30
H-18 wheel; ASTM D-1044.
Tensile Set 70 %
70 %
at break; ASTM D-412
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
DIN/IRC 112