Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan C 70 A HPM TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan C 70 A HPM TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance.Typical Applications: Spiral tubing, pneumatic tubing, round and v-belting, technical moldings, e.g. bushes, dust caps, seals, blow molding bellows, and mining screens.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength 30.0 MPa
4350 psi
after storage in water at 80°C for 42 days; ISO 37
45.0 MPa
6530 psi
ISO 37
1.50 MPa

@Strain 20.0 %
218 psi

@Strain 20.0 %
ISO 37
2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 37
4.50 MPa

@Strain 300 %
653 psi

@Strain 300 %
ISO 37
Elongation at Break 750 %
750 %
ISO 37
850 %
850 %
after storage in water at 80°C for 42 days; ISO 37
Charpy Impact, Notched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
DIN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 40.0 kN/m
228 pli
DIN ISO 34-1/Bb
Abrasion 35
35
[mm<sup>3</sup>; ISO 4649
Compression Set 15 %

@Temperature 23.0 °C
15 %

@Temperature 73.4 °F
ISO 815
25 %

@Temperature 70.0 °C
25 %

@Temperature 158 °F
ISO 815
Processing Properties Metric English Comments
Processing Temperature 160 - 220 °C
320 - 428 °F
Extrusion
170 - 240 °C
338 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding, Extrusion and Blow molding
Users viewing this material also viewed the following: