| Category | Polymer , Film , Thermoplastic , Nylon |
| Manufacturer | BASF |
| Trade Name | Ultramid® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | |
| Water Vapor Transmission | 25.0 g/m²/day | 1.61 g/100 in²/day | 85% RH |
| Oxygen Transmission Rate | 14.0 cc/m²/day | 0.902 cc/100 in²/day | 50% RH |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 70.0 MPa | 10200 psi | TD |
| 70.0 MPa | 10200 psi | MD | |
| Elongation at Break | 475 % | 475 % | MD |
| 480 % | 480 % | TD | |
| Tensile Modulus | 0.600 GPa | 87.0 ksi | TD |
| 0.600 GPa | 87.0 ksi | MD |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 189 °C | 372 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Commercial Status | Europe | |
| Film Grade | 1-3 | BASF |
| Lubricant | 250 - 550 mg/kg | BASF |