Material Notes:
PEEK-CF30Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption 0.040 %
0.040 %
similar to ISO 62 test
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Modulus 23.5 GPa
3410 ksi
ISO 527-1
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 0.650 J/cm²
3.09 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 310 °C
590 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
IEC 60093
Descriptive Properties Value Comments
Resin Type PEEK-CF30