Material Notes:
Description: High flexural modulus, excellent mold release, antistatic.Applications: Suggested uses include intricately designed parts, thin-walled parts, dairy containers.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 100 g/10 min

@Load 2.16 kg,
Temperature 230 °C
100 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength 25.5 MPa
3700 psi
2 in/min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2 in/min; ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256A