Gwent Electronic Materials C2030519P5 Carbon Graphite Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2030519P5 Carbon Graphite Ink.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This Carbon Graphite Ink is designed to be used for screen printing working electrodes. These electrodes when used in conjunction with NAD+/NADH dependent dehydrogenase enzymes, enable the detection of many analytes. The ink contains Meldola’s Blue mediator and it has been optimised to give superior electrochemical performance for NADH detection at potential close to 0V. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156-230tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 38 - 42 %

@Temperature 130 °C
38 - 42 %

@Temperature 266 °F
Viscosity 2000 - 5500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
2000 - 5500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 270
Using a 230 mesh stainless steel screen