CMW® ELKONITE® 10W53 Heat Treatable Copper Tungsten

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® 10W53 Heat Treatable Copper Tungsten.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: Resistance / projection welding electrodesInformation provided by CMW Inc.
Physical Properties Metric English Comments
Density 14.79 g/cc
0.5343 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 109
109
Flexural Modulus 1.38 GPa
200 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
Melting Point <= 3410 °C
<= 6170 °F
Liquidus 3410 °C
6170 °F
Component Elements Properties Metric English Comments
Copper, Cu 24.11 %
24.11 %
Nickel, Ni 0.69 %
0.69 %
Silicon, Si 0.20 %
0.20 %
Tungsten, W 75 %
75 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000616 ohm-cm
0.00000616 ohm-cm
(28% IACS)