Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carlson C 600ESR Nickel-Chromium-Iron Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Carlson
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carlson C 600ESR Nickel-Chromium-Iron Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to chloride-ion stress corrosion cracking and imparts resistance to corrosion by a number of organic and inorganic compounds. Chromium gives this alloy its resistance to oxidation at temperatures up to 2150°F (1175°C).C 600 combines high strength with desirable workabi8lity. It has excellent mechanical properties from sub-zero to elevated temperatures.ApplicationsChemical Processing – calcium and magnesium chloride production; hydrofluoric acid processes; catalyst support equipment in nitric acid production; ammonia converters; tubing, bends and flanges in vinylchloride production; fluorination reactors; fatty acid vessels; and chlorination equipment.Pulp and Paper – liquid heater tubing for pulp digesters; reactors and piping for disposal of organic wastes; sulfate and soda digester liningsOre Processing – chlorine preheaters for zirconium and titanium production; cans for purification of zirconium salts; titanium dioxide production; reactors for manufacturing aluminum fluoride.Food Processing – vegetable processing equipmentThermal Processing – equipment for heat treating muffles, retorts, baskets and boxes, furnace fixtures and radiant tubing.Power Generation – nuclear reactors components and steam-turbine crossover bellows.Information provided by Carlson
Physical Properties Metric English Comments
Density 8.42 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 552 MPa
>= 80000 psi
Tensile Strength, Yield >= 241 MPa

@Strain 0.200 %
>= 35000 psi

@Strain 0.200 %
Elongation at Break >= 30 %
>= 30 %
Modulus of Elasticity 207 GPa
30000 ksi
Tension
Poissons Ratio 0.36
0.36
Calculated
Shear Modulus 75.8 GPa
11000 ksi
Thermal Properties Metric English Comments
CTE, linear 13.3 µm/m-°C

@Temperature 21.1 - 93.3 °C
7.40 µin/in-°F

@Temperature 70.0 - 200 °F
14.2 µm/m-°C

@Temperature 21.1 - 316 °C
7.90 µin/in-°F

@Temperature 70.0 - 600 °F
15.5 µm/m-°C

@Temperature 21.1 - 649 °C
8.60 µin/in-°F

@Temperature 70.0 - 1200 °F
16.7 µm/m-°C

@Temperature 21.1 - 982 °C
9.30 µin/in-°F

@Temperature 70.0 - 1800 °F
Specific Heat Capacity 0.444 J/g-°C
0.106 BTU/lb-°F
Melting Point 1350 - 1413 °C
2470 - 2575 °F
Solidus 1350 °C
2470 °F
Liquidus 1413 °C
2575 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 14 - 17 %
14 - 17 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe 6.0 - 10 %
6.0 - 10 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni >= 72 %
>= 72 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.015 %
<= 0.015 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000103 ohm-cm
0.000103 ohm-cm
Magnetic Permeability 1.01
1.01
200 Oersted
Curie Temperature -124.4 °C
-191.9 °F
Users viewing this material also viewed the following: