Chase Plastics CP Pryme® PC300RUV Polycarbonate (Utility Grade), UV Stabilizer, Mold Release

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chase Plastics CP Pryme® PC300RUV Polycarbonate (Utility Grade), UV Stabilizer, Mold Release.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
ASTM D648