Material Notes:
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light-colored products. Applications requiring flex life coupled with good flexibility at low temperatures, such as hose, railway tie pads and snowboard boot heel, etc. For blending with PVC to improve the mechanical properties.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Melt Flow 5.0 - 7.0 g/10 min
5.0 - 7.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ISO 868
Tensile Strength, Ultimate 25.0 MPa
3630 psi
ISO 527-1
Elongation at Break 540 %
540 %
ISO 527-1
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Tear Strength 95.0 kN/m
542 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974