Colorite Polymers Weatherflex™ CS1521WX (NTL01B) Wire and Cable Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Colorite Polymers
Trade Name Weatherflex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers Weatherflex™ CS1521WX (NTL01B) Wire and Cable Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are available in UL and non-UL grades. In addition, the engineering-grade thermoplastic elastomers we offer can stand up to the most demanding applications . . . while providing the most desirable performance characteristics at a cost that’s more affordable than “ordinary” elastomers.Typical Applications: Class 36 TPE non-leaded jacket for flexible cords.Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Loss On Ignition 31 %
31 %
ASTM 2863
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
10 sec; ASTM D2240
Tensile Strength, Ultimate 13.9 MPa
2010 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Brittleness Temperature -66.0 °C
-86.8 °F
ASTM D746