| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | CoorsTek |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | CoorsTek PlasmaPure-UC™ 99.9% Alumina.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.94 g/cc | 0.142 lb/in³ | ASTM-C 20 |
| Particle Size | 3.0 µm | 3.0 µm | Average Crystal Size; THIN-SECTION |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell 45 N | 85 | 85 | |
| Modulus of Elasticity | 386 GPa | 56000 ksi | ASTM-C848 |
| Flexural Strength | 414 MPa | 60000 psi | MOR; ASTM-F417 |
| Compressive Strength | 2930 MPa | 425000 psi | ASTM-C773 |
| Poissons Ratio | 0.24 | 0.24 | ASTM-C848 |
| Fracture Toughness | 4.00 - 5.00 MPa-m½ | 3.64 - 4.55 ksi-in½ | Klc; Notched Beam |
| Shear Modulus | 156 GPa | 22600 ksi | Calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 8.20 µm/m-°C @Temperature 25.0 - 1000 °C |
4.56 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM-C372 |
| Thermal Conductivity | 31.0 W/m-K | 215 BTU-in/hr-ft²-°F | ASTM-C408 |
| Maximum Service Temperature, Air | 1750 °C | 3180 °F | NO-LOAD COND. |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | >= 99.9 % | >= 99.9 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.10e+7 ohm-cm @Temperature 1000 °C |
1.10e+7 ohm-cm @Temperature 1830 °F |
ASTM-D1829 |
| 3.30e+12 ohm-cm @Temperature 500 °C |
3.30e+12 ohm-cm @Temperature 932 °F |
ASTM-D1829 | |
| >= 1.00e+14 ohm-cm @Temperature 25.0 °C |
>= 1.00e+14 ohm-cm @Temperature 77.0 °F |
ASTM-D1829 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Ivory | |
| Thermal Shock Resistance (°C) | 200 | ΔTc |