| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnitel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Arnitel® PB420 TPC-ET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| Melt Flow | 10 g/10 min @Load 10.0 kg, Temperature 230 °C |
10 g/10 min @Load 22.0 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 38 @Time 3.00 sec |
38 @Time 0.000833 hour |
ISO 868 |
| Tensile Strength, Ultimate | 19.0 MPa | 2760 psi | ISO 527-1/-2 |
| Tensile Stress | 3.70 MPa @Strain 5.00 % |
537 psi @Strain 5.00 % |
ISO 527-1/-2 |
| 6.20 MPa @Strain 10.0 % |
899 psi @Strain 10.0 % |
ISO 527-1/-2 | |
| 12.2 MPa @Strain 50.0 % |
1770 psi @Strain 50.0 % |
ISO 527-1/-2 | |
| 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 527-1/-2 | |
| Elongation at Break | 170 % | 170 % | ISO 527-1/-2 |
| Tensile Modulus | 0.0700 GPa | 10.2 ksi | ISO 527-1/-2 |
| Izod Impact Resistance | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 180/1A |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 180/1A | |
| Charpy Impact, Notched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eA |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 210 °C | 410 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |