| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET) | 
| Manufacturer | Diamond and Network Polymers | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Diamond Polymers DIAMALOY 627 PC/Polyester Alloy.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 | 
| Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D955 | 
| Melt Flow | 6.2           g/10 min @Load 3.80 kg, Temperature 300 °C | 6.2           g/10 min @Load 8.38 lb, Temperature 572 °F | ASTM D1238 | 
| 26.2           g/10 min @Load 5.00 kg, Temperature 260 °C | 26.2           g/10 min @Load 11.0 lb, Temperature 500 °F | ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 51.7 MPa | 7500 psi | chs 2.0 in/min; ASTM D638 | 
| Elongation at Yield | 4.5 % | 4.5 % | chs 2.0 in/min; ASTM D638 | 
| Flexural Yield Strength | 73.0 MPa | 10600 psi | chs 0.05 in/min; ASTM D790 | 
| Flexural Modulus | 1.998 GPa | 289.8 ksi | chs 0.05 in/min; ASTM D790 | 
| Izod Impact, Notched | 6.94           J/cm @Thickness 3.17 mm | 13.0           ft-lb/in @Thickness 0.125 in | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Vicat Softening Point | 161           °C @Load 1.00 kg, Thickness 3.17 mm | 322           °F @Load 2.20 lb, Thickness 0.125 in | ASTM D1527 |