Diamond Polymers DIAMALOY 730 ABS/PC Alloy, Flame Retardant

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 730 ABS/PC Alloy, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 260 °C
10 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.415 GPa
350.3 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 5.30 J/cm

@Thickness 3.17 mm
9.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in