Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 34.5 MPa
5000 psi
chs 2.0 in/min; ASTM D638
Elongation at Yield 12 %
12 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 1.171 GPa
169.8 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.599 ft-lb/in

@Thickness 0.125 in
ASTM D256