Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792-91 |
Multibase Multi-Flex® TPO D 3105 The following is the actual data obtained from the above sample number. This material is based on new generation TPO technology. It has been designed for use as the first shot for airbag covers.Da.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 30-0300 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 30-0400 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 30-0500 A Description: Homopolymer Polypropylene with AntistaticInformation provided by Network Polymers Inc. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 30-1800 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Phillips 66 COPYLENE® CH003T Polypropylene, Homopolymer, Sheet COPYLENE™ CH003T, a fractional melt flow polypropylene homopolymer resin, is available in pellet form. Replacement alternative for Pro-fax® HL561CInformation provided by Phillips 66. |
|||
Density | 0.904 - 0.908 g/cc | 0.0327 - 0.0328 lb/in³ | ASTM D1505 |
Ineos H20Z-03 Polypropylene Homopolymer This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520... |
|||
Density | 0.904 - 0.908 g/cc | 0.0327 - 0.0328 lb/in³ | ASTM D1505 |
Ineos H36G-00 Polypropylene Homopolymer This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 .. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 6001 BLK TPE A 6001 is designed for gasket seals, rotational valves, and electrical applications as well as low friction applications. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis BC650MO Polypropylene Copolymer BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis BH345MO Polypropylene Copolymer BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis BJ100HP Polypropylene Copolymer BJ100HP is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wi.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D1505 |
UBE UMERIT 500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® P353 Polymer Modifier DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Diamond Polymers NPP30-0500 Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Bapolene® PP5072 Polypropylene, Injection Grade Bapolene PP 5072 is a multipurpose, high flow impact copolymer with excellent color and processability. This resin also exhibits a superior balance of stiffness and impact strength. This product m.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | |
BASF BAPMA N,N-Bis-(3-aminopropyl)methylamine Formula: C7H18N3CAS: 105-83-9Description: N,N-Bis-(3-aminopropyl)methylamine is a colorless to yellow liquid, with an amine-like odor. It is miscible with water in all proportion.Synonyms: BAPMA, M.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade Bapolene PP4022 is a PP homopolymer designed for oriented film applications. It offers good clarity and optical properties. This resin meets FDA standards for food contact applications.Application.. |
|||
Density | 0.904 - 0.908 g/cc | 0.0327 - 0.0328 lb/in³ | ASTM D1505 |
Ineos H03G-01 Polypropylene Homopolymer This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrap.. |
|||
Density | 0.904 g/cc | 0.0327 lb/in³ | ASTM D792 |
Ineos H20E-00 Polypropylene Homopolymer This is a homopolymer containing antistatic designed for injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Application.. |