Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow BETAMATE™ 7000/7050 L Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Dow Chemical
Trade Name BETAMATE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAMATE™ 7000/7050 L Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two component room temperature fast curing polyurethane structural adhesive with high elastic modulus.Information provided by Dow
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
DIN 53 504
Tensile Strength, Ultimate >= 28.0 MPa
>= 4060 psi
DIN 53 504
Elongation at Break 3.0 %
3.0 %
DIN 53 504
Modulus of Elasticity 3.10 GPa
450 ksi
DIN 53 504
Adhesive Bond Strength >= 13.0 MPa
>= 1890 psi
Lap Shear Strength; EN 1465
Processing Properties Metric English Comments
Cure Time 960 - 1440 min
16.0 - 24.0 hour