Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DS6D81 Polypropylene Random Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Film Grade
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DS6D81 Polypropylene Random Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
OverviewConsistent processabilityGood optical propertiesLow temperature heat sealComplies with U.S. FDA 21 CFR 177.1520 (c)3.1a, Canadian HPFB No ObjectionDOW DS6D81 Polypropylene Resin is intended for use as a heat seal coating on OPP film.Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus, 1% Secant 550 MPa
79800 psi
ASTM D790A
Izod Impact, Notched 0.907 J/cm
1.70 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
DSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 67.8 °C
154 °F
Unannealed; ASTM D648