Dow TF0807 TPO

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow TF0807 TPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Linear Mold Shrinkage 0.0034 - 0.0044 cm/cm
0.0034 - 0.0044 in/in
Unannealed; ASTM D955
0.0041 - 0.0053 cm/cm
0.0041 - 0.0053 in/in
Annealed; ASTM D955
Melt Flow 14.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.62 MPa
1975 psi
ASTM D638
Tensile Strength, Yield 19.0 MPa
2750 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Elongation at Yield 4.8 %
4.8 %
ASTM D638
Tensile Modulus 1.31 GPa
190 ksi
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
ASTM D790A
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0°F; ASTM D256A
2.35 J/cm
4.40 ft-lb/in
32°F; ASTM D256A
6.78 J/cm
12.7 ft-lb/in
72°F; ASTM D256A
Impact Test 24.9 J
18.3 ft-lb
ID Impact @ 5mph, Peak Energy; ASTM D3763-86
39.5 J
29.2 ft-lb
ID Impact @ 5mph, Total Energy; ASTM D3763-86