| Category | Polymer , Thermoplastic , SAN Polymer |
| Manufacturer | Dow Chemical |
| Trade Name | Tyril® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Tyril® 100 SAN.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM Data |
| Melt Density | 0.978 g/cc | 0.0353 lb/in³ | Melt density |
| Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | |
| Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM Data |
| Tensile Strength, Yield | 69.0 MPa | 10000 psi | ASTM Data |
| Elongation at Break | 2.5 % | 2.5 % | ASTM Data |
| Tensile Modulus | 3.28 GPa | 476 ksi | ASTM Data |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ASTM data |
| Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
| Thermal Conductivity | 0.193 W/m-K | 1.34 BTU-in/hr-ft²-°F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Unannealed; ASTM Data |
| 104 °C | 219 °F | Annealed; ASTM Data | |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F | Unannealed; 102°C (216°F) annealed; ASTM Data |
| Vicat Softening Point | 110 °C | 230 °F | |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
|
| Oxygen Index | 19 % | 19 % |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 0.65 % | 0.65 % | |
| Transmission, Visible | 88.5 % | 88.5 % |