| Category | Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Hytrel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| Water Absorption | 6.8 % @Thickness 2.00 mm |
6.8 % @Thickness 0.0787 in |
Sim. to ISO 62 |
| Moisture Absorption | 0.700 % @Thickness 2.00 mm |
0.700 % @Thickness 0.0787 in |
Sim. to ISO 62 |
| Water Absorption at Saturation | 3.5 % | 3.5 % | Immersion 24h; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 2577 |
| Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 21.0 MPa | 3050 psi | ISO 527-1/-2 |
| Tensile Stress | 4.20 MPa @Strain 10.0 % |
609 psi @Strain 10.0 % |
ISO 527-1/-2 |
| Elongation at Break | >= 300 % | >= 300 % | ISO 527-1/-2 |
| Tensile Modulus | 0.0540 GPa | 7.83 ksi | ISO 527-1/-2 |
| Flexural Modulus | 0.0580 GPa | 8.41 ksi | ISO 178 |
| Charpy Impact, Notched | NB | NB | ISO 179/1eA |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ISO 179/1eA | |
| Tear Strength | 70.0 kN/m | 399 pli | parallel; ISO 34-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 175 °C | 347 °F | 10°C/min; ISO 11357-1/-3 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Delivery Form | Pellets | |
| Part Marking Code | >TPC-ET< | ISO 11469 |
| Processing | Casting | |
| Film Extrusion | ||
| Injection Moulding | ||
| Other Extrusion | ||
| Profile Extrusion | ||
| Sheet Extrusion | ||
| Thermoforming | ||
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | TPC-ET | ISO 1043 |
| Special Characteristics | Light stabilised or stable to light |