DuPont Performance Polymers Zytel® HTN 54G35EF BKB336 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Performance Polymers Zytel® HTN 54G35EF BKB336 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
35% Glass Reinforced  laser markable PPA  High Performance Polyamide Developed for Electrical and Electronics Applications. Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin developedInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 189 MPa
27400 psi
DAM; ISO 527-1/-2
Elongation at Break 2.7 %
2.7 %
DAM; ISO 527-1/-2
Tensile Modulus 11.7 GPa
1700 ksi
DAM; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Part Marking Code >PA-IGF35<
ISO 11469
>PPA-IGF35<
SAE J1344
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Special Characteristics Heat stabilised or stable to heat