| Category | Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® RS |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | DAM; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 40.0 MPa @Temperature 23.0 °C |
5800 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 43.0 MPa @Temperature 23.0 °C |
6240 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Tensile Stress | 0.0300 MPa @Strain 0.000 %, Temperature 40.0 °C |
4.35 psi @Strain 0.000 %, Temperature 104 °F |
DAM; ISO 11403-1/-2 |
| 0.0500 MPa @Strain 0.000 %, Temperature 40.0 °C |
7.25 psi @Strain 0.000 %, Temperature 104 °F |
50%RH; ISO 11403-1/-2 | |
| 0.0600 MPa @Strain 0.000 %, Temperature 60.0 °C |
8.70 psi @Strain 0.000 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 | |
| 0.0700 MPa @Strain 0.000 %, Temperature 23.0 °C |
10.2 psi @Strain 0.000 %, Temperature 73.4 °F |
50%RH; ISO 11403-1/-2 | |
| 0.0800 MPa @Strain 0.000 %, Temperature 60.0 °C |
11.6 psi @Strain 0.000 %, Temperature 140 °F |
50%RH; ISO 11403-1/-2 | |
| 0.0800 MPa @Strain 0.000 %, Temperature 90.0 °C |
11.6 psi @Strain 0.000 %, Temperature 194 °F |
50%RH; ISO 11403-1/-2 | |
| 0.0800 MPa @Strain 0.000 %, Temperature 90.0 °C |
11.6 psi @Strain 0.000 %, Temperature 194 °F |
DAM; ISO 11403-1/-2 | |
| 0.100 MPa @Strain 0.000 %, Temperature 120 °C |
14.5 psi @Strain 0.000 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 | |
| 0.100 MPa @Strain 0.000 %, Temperature 120 °C |
14.5 psi @Strain 0.000 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 | |
| 0.100 MPa @Strain 0.000 %, Temperature 23.0 °C |
14.5 psi @Strain 0.000 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 0.130 MPa @Strain 0.000 %, Temperature 150 °C |
18.9 psi @Strain 0.000 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 0.130 MPa @Strain 0.000 %, Temperature 150 °C |
18.9 psi @Strain 0.000 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 | |
| 0.150 MPa @Strain 0.000 %, Temperature -40.0 °C |
21.8 psi @Strain 0.000 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 0.160 MPa @Strain 0.000 %, Temperature 0.000 °C |
23.2 psi @Strain 0.000 %, Temperature 32.0 °F |
DAM; ISO 11403-1/-2 | |
| 0.200 MPa @Strain 0.000 %, Temperature 0.000 °C |
29.0 psi @Strain 0.000 %, Temperature 32.0 °F |
50%RH; ISO 11403-1/-2 | |
| 0.240 MPa @Strain 0.000 %, Temperature -40.0 °C |
34.8 psi @Strain 0.000 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 0.240 MPa @Strain 0.000 %, Temperature -20.0 °C |
34.8 psi @Strain 0.000 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 | |
| 0.270 MPa @Strain 0.000 %, Temperature -20.0 °C |
39.2 psi @Strain 0.000 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 | |
| 0.420 MPa @Strain 0.0300 %, Temperature -40.0 °C |
60.9 psi @Strain 0.0300 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 0.430 MPa @Strain 0.0200 %, Temperature -40.0 °C |
62.4 psi @Strain 0.0200 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 0.450 MPa @Strain 0.240 %, Temperature 120 °C |
65.3 psi @Strain 0.240 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 | |
| 0.750 MPa @Strain 0.250 %, Temperature 60.0 °C |
109 psi @Strain 0.250 %, Temperature 140 °F |
50%RH; ISO 11403-1/-2 | |
| 0.900 MPa @Strain 0.240 %, Temperature 40.0 °C |
131 psi @Strain 0.240 %, Temperature 104 °F |
50%RH; ISO 11403-1/-2 | |
| 0.910 MPa @Strain 0.0700 %, Temperature -20.0 °C |
132 psi @Strain 0.0700 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 | |
| 0.950 MPa @Strain 0.0600 %, Temperature -20.0 °C |
138 psi @Strain 0.0600 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 | |
| 0.960 MPa @Strain 0.250 %, Temperature 40.0 °C |
139 psi @Strain 0.250 %, Temperature 104 °F |
DAM; ISO 11403-1/-2 | |
| 1.07 MPa @Strain 0.600 %, Temperature 120 °C |
155 psi @Strain 0.600 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 | |
| 1.16 MPa @Strain 0.0600 %, Temperature -40.0 °C |
168 psi @Strain 0.0600 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 1.26 MPa @Strain 0.240 %, Temperature 23.0 °C |
183 psi @Strain 0.240 %, Temperature 73.4 °F |
50%RH; ISO 11403-1/-2 | |
| 1.27 MPa @Strain 0.0700 %, Temperature -40.0 °C |
184 psi @Strain 0.0700 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 1.42 MPa @Strain 0.190 %, Temperature 23.0 °C |
206 psi @Strain 0.190 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 | |
| 1.81 MPa @Strain 0.0900 %, Temperature -40.0 °C |
263 psi @Strain 0.0900 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 1.93 MPa @Strain 0.910 %, Temperature 90.0 °C |
280 psi @Strain 0.910 %, Temperature 194 °F |
50%RH; ISO 11403-1/-2 | |
| 2.07 MPa @Strain 0.100 %, Temperature -40.0 °C |
300 psi @Strain 0.100 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 2.08 MPa @Strain 0.180 %, Temperature 0.000 °C |
302 psi @Strain 0.180 %, Temperature 32.0 °F |
50%RH; ISO 11403-1/-2 | |
| 2.13 MPa @Strain 0.150 %, Temperature -20.0 °C |
309 psi @Strain 0.150 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 | |
| 2.21 MPa @Strain 0.130 %, Temperature -20.0 °C |
321 psi @Strain 0.130 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 | |
| 2.23 MPa @Strain 0.180 %, Temperature 0.000 °C |
323 psi @Strain 0.180 %, Temperature 32.0 °F |
DAM; ISO 11403-1/-2 | |
| 2.60 MPa @Strain 0.130 %, Temperature -40.0 °C |
377 psi @Strain 0.130 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 2.87 MPa @Strain 0.130 %, Temperature -40.0 °C |
416 psi @Strain 0.130 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 3.28 MPa @Strain 4.15 %, Temperature 150 °C |
476 psi @Strain 4.15 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 | |
| 3.33 MPa @Strain 0.160 %, Temperature -40.0 °C |
483 psi @Strain 0.160 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 3.37 MPa @Strain 0.220 %, Temperature -20.0 °C |
489 psi @Strain 0.220 %, Temperature -4.00 °F |
50%RH; ISO 11403-1/-2 | |
| 3.38 MPa @Strain 0.200 %, Temperature -20.0 °C |
490 psi @Strain 0.200 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 | |
| 3.45 MPa @Strain 4.11 %, Temperature 150 °C |
500 psi @Strain 4.11 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 3.59 MPa @Strain 1.28 %, Temperature 60.0 °C |
521 psi @Strain 1.28 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 | |
| 3.66 MPa @Strain 0.170 %, Temperature -40.0 °C |
531 psi @Strain 0.170 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 3.99 MPa @Strain 0.190 %, Temperature -40.0 °C |
579 psi @Strain 0.190 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 4.41 MPa @Strain 0.200 %, Temperature -40.0 °C |
640 psi @Strain 0.200 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 4.68 MPa @Strain 0.210 %, Temperature -40.0 °C |
679 psi @Strain 0.210 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 5.15 MPa @Strain 0.230 %, Temperature -40.0 °C |
747 psi @Strain 0.230 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 | |
| 5.26 MPa @Strain 2.77 %, Temperature 90.0 °C |
763 psi @Strain 2.77 %, Temperature 194 °F |
DAM; ISO 11403-1/-2 | |
| 5.37 MPa @Strain 0.240 %, Temperature -40.0 °C |
779 psi @Strain 0.240 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 | |
| 6.13 MPa @Strain 18.49 %, Temperature 150 °C |
889 psi @Strain 18.49 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 | |
| 6.43 MPa @Strain 18.66 %, Temperature 150 °C |
933 psi @Strain 18.66 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 6.87 MPa @Strain 34.43 %, Temperature 150 °C |
996 psi @Strain 34.43 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 | |
| 7.19 MPa @Strain 34.72 %, Temperature 150 °C |
1040 psi @Strain 34.72 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 | |
| 7.22 MPa @Strain 51.35 %, Temperature 150 °C |
1050 psi @Strain 51.35 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 | |
| 7.48 MPa @Strain 68.02 %, Temperature 150 °C |
1080 psi @Strain 68.02 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 |