DuPont™ Surlyn® 9320W Ionomer Resin, Zinc  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 9320W Ionomer Resin, Zinc  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Surlyn® 9320W thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. This very low modulus zinc grade has low hardness and very low stiffness. Increased flexibility is achieved by incorporating a third co-monomer into the resin during polymerization. The resin can be used alone or in combination with other grades of Surlyn® to provide varying degrees of flexibility, softness and toughness. It can be used as a modifier that yields supertough properties in nylon 6 and 6/6 resins. In golf ball covers, the resin provides a softer feel and imparts greater spin when the ball is in contact with the club face. The resin can be blow molded or extruded into sheets or shapes, but is usually injection molded in blends with other polymers.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.9 MPa
2310 psi
ASTM D638
Elongation at Break 525 %
525 %
ASTM D638
Flexural Modulus 0.0296 GPa
4.29 ksi
ASTM D790
Abrasion 169
169
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
Melting Point 70.0 °C
158 °F
DSC
Vicat Softening Point 48.0 °C
118 °F
Rate B, ASTM D1525-70