Eagle Brass 220 Commercial Bronze, 1/2 Hard

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Eagle Brass 220 Commercial Bronze, 1/2 Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plumbing brass, small arms cartridges, cable wrap, marine hardware, flexible tube, blots, screws, wave guides costume jewelry and kick plates.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 52 - 61
52 - 61
Thickness > 0.020 Inch
Tensile Strength, Ultimate 324 - 393 MPa
47000 - 57000 psi
Tensile Strength, Yield 290 - 365 MPa
42000 - 53000 psi
0.2% offset
Elongation at Break 5.0 - 20 %
5.0 - 20 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.4 µm/m-°C

@Temperature 20.0 - 300 °C
10.2 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 188.5 W/m-K
1308 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 90 %
90 %
Zinc, Zn 10 %
10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000405 ohm-cm
0.00000405 ohm-cm
Annealed