| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.86 g/cc | 0.320 lb/in³ | Annealed |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 758 - 862 MPa | 110000 - 125000 psi | |
| Tensile Strength, Yield | >= 689 MPa | >= 100000 psi | 0.2% offset |
| Elongation at Break | >= 1.0 % | >= 1.0 % | in 2 in. |
| Tensile Modulus | 131 GPa | 19000 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 300 °C |
10.0 µin/in-°F @Temperature 68.0 - 572 °F |
|
| Thermal Conductivity | 15.6 W/m-K | 108 BTU-in/hr-ft²-°F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 97 % | 97 % | |
| Nickel, Ni | 2.0 % | 2.0 % | |
| Silicon, Si | 0.40 % | 0.40 % | |
| Tin, Sn | 0.42 % | 0.42 % | |
| Zinc, Zn | 0.30 % | 0.30 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00000445 ohm-cm | 0.00000445 ohm-cm | Annealed |