ExxonMobil Bicor® 30 ARW OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor® 30 ARW OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher COF is intended to be against the paper to ensure a tight wrap, where as the side with the lower COF is intended as the outside surface. This film has a broad has a broad seal range suitable for ream overwrap applications.Availability: Latin America, North America and South AmericaKey Features:Consistent COFRobust machinablityExcellent optical propertiesGood hot slipExcellent stiffnessExcellent hot melt adhesionExcellent hot tack and seal strengthExcellent flavor and aroma barrierFeatures:Acrylic CoatedBroad Seal RangeIn Lamination Lap SealableApplications:Paper Ream wrapUses:Box Overwrap Flexible PackagingHFF Flexible PackagingPre-made Bags - Flexible PackagingTobacco Overwrap Flexible PackagingVFFS Flexible PackagingProcessing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination and Surface Print Unsupported Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 5.00 g/m²/day
0.322 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
Coating Weight 26.6 g/m²
16.6 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.25
0.25
Slip Modified/Slip Modified; ExxonMobil Method
0.52
0.52
Print/Print; ExxonMobil Method
Film Tensile Strength at Break, MD 138 MPa
20000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 234 MPa
34000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %
5.0 %
at 275°F; ExxonMobil Method
Shrinkage, TD 3.5 %
3.5 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
ExxonMobil Method
Gloss 86 %
86 %
45º; ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 185°F
Acrylic/Acrylic
Crimp Seal Strength 500 g/in
260°F, 20psi, 3/4sec
Yield 26100 in2/lb