Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ BMV 301 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ BMV 301 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high scratch resistance and good UV resistance are required.Availability: Asia Pacific, Europe and North America Features: Good Flow Good Impact ResistanceGood StiffnessGood Surface FinishGood UV ResistanceHigh Scratch Resistance Uses: Automotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183/A
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ISO 527-2
Tensile Strength, Yield 21.0 MPa
3050 psi
ISO 527-2
Tensile Modulus 2.03 GPa
294 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.294 J/cm²

@Temperature -30.0 °C
1.40 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
2.10 J/cm²

@Temperature 22.8 °C
10.0 ft-lb/in²

@Temperature 73.0 °F
Partial Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 53.9 °C
129 °F
ISO 75-2/A