| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 15.0 MPa | 2180 psi | ISO 527-2/50 |
| Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-2/50 |
| Elongation at Break | 35 % | 35 % | ISO 527-2/50 |
| Elongation at Yield | 4.0 % | 4.0 % | ISO 527-2/50 |
| Tensile Modulus | 2.95 GPa | 428 ksi | Secant; ISO 527-2/50 |
| Charpy Impact, Notched | 0.399 J/cm² @Temperature 0.000 °C |
1.90 ft-lb/in² @Temperature 32.0 °F |
Complete Break; ISO 179 |
| 1.01 J/cm² @Temperature 22.8 °C |
4.80 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ISO 75-2/B |