Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Exxtral™ LNT 010 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ LNT 010 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with high heat ageing resistance, high transparency, low color and low discoloration for contact with hot water, hot air and detergent in electrical appliances such as washing machines.Availability: Availability: Africa & Middle East, Asia Pacific, Europe, North America and South America Features:Good Mold ReleaseGood Surface FinishGood Thermal Stability Uses: Appliance ComponentsAppliancesAutomotive ApplicationsAutomotive Under the HoodConsumer ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-2/50
Elongation at Break >= 200 %
>= 200 %
ISO 527-2/50
Elongation at Yield 10 %
10 %
ISO 527-2/50
Tensile Modulus 1.40 GPa
203 ksi
Secant; ISO 527-2
Flexural Modulus 1.35 GPa
196 ksi
ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2/A
Vicat Softening Point 81.1 °C
178 °F
ISO 306/B50