Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

GEHR Plastics PE-UHMW-ELS Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF GEHR Plastics PE-UHMW-ELS Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +194 °F. Main Characteristics: light weight; high chemical resistance; high toughness (also at low temperature); good protection against stress cracking; high elongation; food safe; very good electrical and dielectric properties; soft surface (low tensile strength); HF welding not recommended; very low water absorption • difficult to varnish and glue; low steam permeability; not weather resistantInformation provided by GEHR Plastics, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Ball Indentation Hardness 38.0 MPa
5510 psi
ISO 2039
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Break >= 50 %
>= 50 %
ISO 527
Elongation at Yield 8.0 %
8.0 %
ISO 527
Modulus of Elasticity 0.800 GPa
116 ksi
ISO 527
Izod Impact, Unnotched (ISO) NB
NB
ISO 179
Coefficient of Friction 0.18

@Temperature 60.0 °C
0.18

@Temperature 140 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.400 W/m-K

@Temperature 20.0 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
DIN 52612
Maximum Service Temperature, Air 90.0 °C
194 °F
Vicat Softening Point 76.0 °C
169 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -150 °C
-238 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
VDE 0303
Surface Resistivity per Square 1.00e+7 ohm
1.00e+7 ohm
VDE 0303
Descriptive Properties Value Comments
Acid Resistance Yes
Aromatic Resistance Limited
Bondability No
CKW Resistance No
Hydrocarbonate Resistance Yes
Hydroxide Resistance Yes
Ketone Resistance Yes
Resistance to Hot Water No
UV Stabilization Limited
Copyright © lookpolymers.com All Rights Reserved