ExxonMobil Exxtral™ LNV 010 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ LNV 010 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A specialty thermoplastic polyolefin resin with high gloss, low warpage, and low discoloration in contact with hot water/steam in large electrical appliance such as washing machines. Contains anti-static additive.Availability: Africa & Middle East, Asia Pacific, Europe, North America and South America Features:Good Mold ReleaseGood Surface FinishHigh Flow Uses: Appliance ComponentsAppliances Consumer ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.897 g/cc
0.0324 lb/in³
ISO 1183
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.7 MPa
5030 psi
ISO 527-2/50
Elongation at Yield 7.0 %
7.0 %
ISO 527-2/50
Tensile Modulus 1.60 GPa
232 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.130 J/cm²

@Temperature -30.0 °C
0.620 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.231 J/cm²

@Temperature 22.8 °C
1.10 ft-lb/in²

@Temperature 73.0 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.2 °C
198 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F
ISO 75-2/A
Vicat Softening Point 153 °C
307 °F
ISO 306/A50