Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO), Film Grade
Manufacturer Exxon Chemical
Trade Name Vistamaxx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to process and is compatible with a wide variety of hydrocarbon based polymers. It is available as free flowing pellets.Key Features:Suitable for a wide range of blown and cast film applications, extrusion coating and lamination applications.Excellent adhesion to conventional or metallocene PP and PE.Very good elasticity, toughness and clarity.Very low seal initiation temperature combined with high seal strength when used as sealing layer of co-extruded structures.Very good chemical resistance and long term aging.EU and China RoHS compliant.Applications:Blown FilmCast FilmInjection MoldingCalendered SheetingExtruded SheetingPP/TPO ModificationUses:CompoundingFilmPackagingAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.873 g/cc
0.873 g/cc
ASTM D1505
Melt Flow 8.0 g/10 min
8.0 g/10 min
melt flow rate data; ExxonMobil Method
3.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore D 33

@Time 15.0 sec
33

@Time 0.00417 hour
ASTM D2240
Tensile Stress 4.50 MPa

@Strain 300 %
653 psi

@Strain 300 %
ASTM D412
4.60 MPa

@Strain 100 %
667 psi

@Strain 100 %
ASTM D412
Tensile Strength, Yield 4.90 MPa
711 psi
ASTM D412
Elongation at Yield 48 %
48 %
ASTM D412
Flexural Modulus, 1% Secant 59.3 MPa
8600 psi
ASTM D790
Tear Strength 62.4 kN/m
356 pli
Die C; ASTM D624
Tensile Set 54 %
54 %
ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 65.5 °C
150 °F
ASTM D1525
Descriptive Properties Value Comments
Ethylene Content 11.0 wt%
ASTM D3900
Users viewing this material also viewed the following: