Fibre Glast 1099 Room Temperature Epoxy Surface Coat

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Fibre Glast Developments Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fibre Glast 1099 Room Temperature Epoxy Surface Coat.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that can be used with several hardeners for a range of cured and handling characteristics. #1099 is a versatile material, and will perform well in a variety of room temperature applications. #1099 produces excellent reproduction of very fine detailed surfaces. it is often chosen for broad, flat tooling surfaces, where it can be applied fast. #1099 has been formulated to provide good bonds to subsequently applied layers of epoxy. This feature provides good intercoat bonds, even if the previous layer of #1099 has cured completely hard. This elimination of surface coat adhesion failures is accomplished with no sacrifice in properties. #1099 is an excellent material for all types of general tooling uses.Information provided by Fibre Glast Developments Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
ASTM D2240
Tensile Strength at Break 37.9 MPa
5500 psi
ASTM D638
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Compressive Yield Strength 82.7 MPa
12000 psi
ASTM D695
Processing Properties Metric English Comments
Cure Time 1080 - 1440 min

@Temperature 25.0 °C
18.0 - 24.0 hour

@Temperature 77.0 °F
Pot Life 20 - 25 min
20 - 25 min
Descriptive Properties Value Comments
Color Light Oxide Red
Mix Ratio 100:11
Resin:Hardener by Weight