Material Notes:
Flame retardant polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Melt Flow 19.5 - 20.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
19.5 - 20.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 2.35 GPa
341 ksi
ASTM D790
Izod Impact, Notched 3.92 J/cm
7.35 ft-lb/in
ASTM D256 A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ASTM D648
Flammability, UL94 V-0
V-0