Greene Tweed CHEMRAZ® 584 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 584 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Greene Tweed’s Chemraz® 584, a cream-colored perfluoroelastomer, is a specialty compound formulated to outlast the most demanding chemical process applications. Because of its outstanding overall chemical resistance, Chemraz 584 is the elastomer of choice for chlorine, ozone, strong oxidation fluids and hot aqueous solutions. Its recommended temperature range is -22°F to 428°F (-30°C to 220°C).This unique compound is perfect for applications where contamination from carbon black must be preventedChemraz components are available for use as O-rings, gaskets and many other custom shapes.Applications: Mechanical sealsValvesPump HousingsSampling/metering equipment ReactorsMixersControls/instrumentationInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
ASTM D1414
Tensile Strength, Yield 2.41 MPa
350 psi
@50% Elongation; ASTM D1414
5.38 MPa
780 psi
@100% Elongation; ASTM D1414
Elongation at Break 145 %
145 %
ASTM D1414
Compression Set 35 %
35 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color Cream