H.C. Starck WCu 90/10 Tungsten-Copper Composite Material

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer H.C. Starck
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck WCu 90/10 Tungsten-Copper Composite Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A thermal conductivity over 200 W/m K is producible.Range of Application: Switching contacts for high-voltage and medium-voltage, heat sinks for passive thermal management, electrodes for erosive processing.Information provided by H.C. Starck.
Physical Properties Metric English Comments
Density 17.0 - 17.6 g/cc
0.614 - 0.636 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 220 - 290

@Load 62.5 kg
220 - 290

@Load 138 lb
2.5 mm ball
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
Modulus of Elasticity 340 GPa
49300 ksi
Thermal Properties Metric English Comments
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 100 °C
3.39 µin/in-°F

@Temperature 68.0 - 212 °F
6.40 µm/m-°C

@Temperature 20.0 - 300 °C
3.56 µin/in-°F

@Temperature 68.0 - 572 °F
6.70 µm/m-°C

@Temperature 20.0 - 450 °C
3.72 µin/in-°F

@Temperature 68.0 - 842 °F
Thermal Conductivity 130 - 200 W/m-K
902 - 1390 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 8.0 - 12 %
8.0 - 12 %
Tungsten, W 88 - 92 %
88 - 92 %
Electrical Properties Metric English Comments
Volume Resistivity 0.0000052 ohm-cm
0.0000052 ohm-cm