Material Notes:
A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray.
Physical Properties Metric English Comments
Density 1.87 g/cc
0.0676 lb/in³
ASTM D572
Water Absorption 0.20 %
0.20 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 60
60
Tensile Strength, Ultimate 69.0 MPa
10000 psi
Flexural Strength 159 MPa
23100 psi
Compressive Strength 207 MPa
30000 psi
Izod Impact, Notched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Dielectric Strength 14.0 kV/mm
356 kV/in
Perpendicular (ASTM D149), in Oil
Arc Resistance 150 sec
150 sec
ASTM D495