| Category | Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive |
| Manufacturer | Henkel |
| Trade Name | Hysol |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Henkel Hysol EA 9320NA Paste Adhesive System.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Storage Temperature | 25.0 °C | 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 34.5 MPa | 5000 psi | |
| Elongation at Break | 9.0 % | 9.0 % | |
| Tensile Modulus | 2.28 GPa | 331 ksi | |
| Compressive Strength | 60.7 MPa | 8800 psi | |
| Compressive Modulus | 1.82 GPa | 264 ksi | |
| Adhesive Bond Strength | 6.90 MPa @Temperature 93.0 °C |
1000 psi @Temperature 199 °F |
Tensile Lap Shear |
| 23.5 MPa @Temperature -55.0 °C |
3410 psi @Temperature -67.0 °F |
Tensile Lap Shear | |
| 31.7 MPa @Temperature 25.0 °C |
4600 psi @Temperature 77.0 °F |
Tensile Lap Shear | |
| Peel Strength | 6.00 kN/m | 34.2 pli | Bell Peel |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | >= 82.0 °C | >= 180 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 60.0 min @Temperature 82.0 °C |
1.00 hour @Temperature 180 °F |
|
| 7200 - 10100 min @Temperature 25.0 °C |
120 - 168 hour @Temperature 77.0 °F |
||
| Pot Life | 25 min | 25 min |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Consistency | Moderate Viscosity | |
| Form | 2 parts | |
| Mix Ratio, Part A:Part B | 100:19 | |
| Peel Strength | Moderate |