Material Notes:
Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding
Physical Properties Metric English Comments
Storage Temperature 4.00 °C
39.2 °F
Mechanical Properties Metric English Comments
Tensile Strength 56.6 MPa
8210 psi
Elongation at Break 2.5 %
2.5 %
Tensile Modulus 2.90 GPa
421 ksi
Compressive Strength 36.6 MPa
5310 psi
compressive shear strength as a wet lay-up resin with 3K-70-P fiber
Adhesive Bond Strength 15.2 MPa

@Temperature -55.0 °C
2200 psi

@Temperature -67.0 °F
Tensile Lap Shear
20.7 MPa

@Temperature 93.0 °C
3000 psi

@Temperature 199 °F
Tensile Lap Shear
24.1 MPa

@Temperature 25.0 °C
3500 psi

@Temperature 77.0 °F
Tensile Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 177 °C
>= 351 °F
Processing Properties Metric English Comments
Cure Time 210 min

@Temperature 93.0 °C
3.50 hour

@Temperature 199 °F
Pot Life 120 min
120 min
Descriptive Properties Value Comments
Consistency Low Viscosity
Form 2 parts
Mix Ratio, Part A:Part B 100:56
Peel Strength Nil