Material Notes:
Features:High Strength GradeHigh Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.1 MPa
6250 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 71.7 MPa
10400 psi
ASTM D790
Flexural Modulus 2.94 GPa
427 ksi
ASTM D790
Izod Impact, Notched 0.180 J/cm
0.337 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F
ASTM D648
Vicat Softening Point 96.1 °C
205 °F
ASTM D1525