| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 87 | 87 | Cured; ASTM D2240 |
| Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
| Elongation at Break | <= 300 % | <= 300 % | ASTM D412 |
| Tear Strength | 49.1 kN/m | 280 pli | ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 300 | 300 | H-18 wheel (1000 gram load) |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
| 82.2 °C | 180 °F | dry | |
| Shrinkage | 0.14 % | 0.14 % | Cured; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 720 min | 12.0 hour | Functional cure |
| Pot Life | 25.0 min @Temperature 23.9 °C |
25.0 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per pound, in² @ 1/4" thickness | 94 | |
| Mix ratio by weight (Resin:Hardener) | 72:28 |