| Category | Polymer , Adhesive , Thermoset |
| Manufacturer | ITW Devcon |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.23 g/cc | 0.0806 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 | 85 | Cured; ASTM D2240 |
| Tensile Strength at Break | 23.0 MPa | 3340 psi | ASTM D638 |
| Modulus of Elasticity | 5.52 GPa | 800 ksi | ASTM D638 |
| Flexural Strength | 36.4 MPa | 5280 psi | ASTM D790 |
| Compressive Strength | 57.9 MPa | 8400 psi | ASTM D695 |
| Adhesive Bond Strength | 16.44 MPa | 2385 psi | tensile shear; ASTM D1002 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 61.2 µm/m-°C @Temperature 20.0 °C |
34.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Thermal Conductivity | 0.515 W/m-K | 3.57 BTU-in/hr-ft²-°F | ASTM C177 |
| Maximum Service Temperature, Air | 121 °C | 250 °F | dry |
| Shrinkage | 0.10 % | 0.10 % | Cured; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 75 @Frequency 1000 Hz |
75 @Frequency 1000 Hz |
ASTM D150 |
| Dielectric Strength | 1.18 kV/mm | 30.0 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 960 min | 16.0 hour | Functional cure |
| Pot Life | 58.0 min @Temperature 23.9 °C |
58.0 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per pound, in² @ 1/4" thickness | 50 | |
| Mix ratio by volume (Resin:Hardener) | 3.75:1 | |
| Mix ratio by weight (Resin:Hardener) | 11:1 |