| Category | Polymer , Adhesive , Thermoset , Polyurethane, TS |
| Manufacturer | ITW Devcon |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0442 lb/in³ | |
| Viscosity | 10000 cP | 10000 cP | Mixed Viscosity |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 83 | 83 | Cured; ASTM D2240 |
| Tensile Strength at Break | 17.9 MPa | 2600 psi | ASTM D412 |
| Elongation at Break | <= 800 % | <= 800 % | ASTM D412 |
| Tear Strength | 57.0 kN/m | 325 pli | ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
| 82.2 °C | 180 °F | dry | |
| Shrinkage | 0.14 % | 0.14 % | Cured; ASTM D2566 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 11.8 kV/mm | 300 kV/in | ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min | 2.00 hour | Functional cure |
| Pot Life | 10.0 min @Temperature 23.9 °C |
10.0 min @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Coverage per pound, in² @ 1/4" thickness | 90 | |
| Mix ratio by weight (Resin:Hardener) | 63:37 |