Imerys Kaolexâ„¢ FG Kaolin

Category Ceramic , Clay , Kaolin Clay
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Kaolex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Kaolexâ„¢ FG Kaolin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Kaolex FG is a air floated Hydrated Aluminum Silicate. Its low surface area makes it a good choice for fiberglass manufacturing.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 70 - 90 %
70 - 90 %
% Reflectance
Particle Size 1.1 µm
1.1 µm
average
Particle Mesh Size 60 Mesh
60 Mesh
0.05% retained
325 Mesh
325 Mesh
1.01% retained
pH 4.0 - 5.5
4.0 - 5.5
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Descriptive Properties Value Comments
Heating Loss (% max as produced) 1
at 105°C