| Category | Ceramic , Clay , Kaolin Clay |
| Manufacturer | Imerys (Kentucky-Tennessee Clay Co.) |
| Trade Name | Kingsley - Rogers™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Imerys Kingsley - Rogersâ„¢ Kaolin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | 0.50 µm | 0.50 µm | 34% finer than |
| 1.0 µm | 1.0 µm | 49% finer than | |
| 2.0 µm | 2.0 µm | 62% finer than | |
| 5.0 µm | 5.0 µm | 80% finer than | |
| 10 µm | 10 µm | 90% finer than | |
| 20 µm | 20 µm | 97% finer than | |
| pH | 4.5 - 6.5 | 4.5 - 6.5 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 0.00345 GPa | 0.500 ksi | dry |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 38.1 % | 38.1 % | |
| CaO | 0.10 % | 0.10 % | |
| Fe2O3 | 0.60 % | 0.60 % | |
| K2O | 0.20 % | 0.20 % | |
| Loss on Ignition(%) | 13.6 % | 13.6 % | |
| MgO | 0.10 % | 0.10 % | |
| Na2O | 0.10 % | 0.10 % | |
| SiO2 | 45.1 % | 45.1 % | |
| TiO2 | 1.7 % | 1.7 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| M.B.I. (meq/100g) | 4.6 |