Indium Corp. Indalloy 120 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 120 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.95 g/cc
0.323 lb/in³
Thermal Properties Metric English Comments
Melting Point 183 - 218 °C
361 - 424 °F
Solidus 183 °C
361 °F
Liquidus 218 °C
424 °F
Component Elements Properties Metric English Comments
Lead, Pb 52 %
52 %
Tin, Sn 48 %
48 %