| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | DIN 53479 |
| Water Absorption | 0.30 - 0.50 % | 0.30 - 0.50 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 80 | 80 | ASTM D785 |
| Hardness, Shore D | 60 | 60 | DIN 53505 |
| Tensile Strength | 0.300 - 0.390 MPa | 43.5 - 56.6 psi | DIN 53455 |
| Elongation at Break | 200 - 800 % | 200 - 800 % | DIN 53455 |
| Tensile Modulus | 0.00800 - 0.700 GPa | 1.16 - 102 ksi | DIN 53457 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 160 - 190 µm/m-°C | 88.9 - 106 µin/in-°F | DIN 52328 |
| Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous; DIN 52612 |
| Minimum Service Temperature, Air | -70.0 °C | -94.0 °F | Continuous; DIN 52612 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.4 - 7.1 @Frequency 1000 Hz |
3.4 - 7.1 @Frequency 1000 Hz |
DIN 53483 |
| Dielectric Strength | 14.0 - 26.0 kV/mm | 356 - 660 kV/in | DIN 53481 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Several Colors |